Nanoindent. An AFM image of the residual indent left by Berkovitch tip during nanoindentation experiment on ZrCuAl metallic glass Image by Jonathan Puthoff University of Wisconsin Madison en Jputhoff en Jputhoff original upload log page en Nanoindent Jputhoff bytes no AFM image of the residual indent left by Berkovitch